| 文档摘要:针对高钛超低碳搪瓷钢可浇性差、水口易结瘤情况,对水口结瘤物和结瘤原因进行了机理分析.后续通过强化钢包顶渣改质,降低了顶渣氧化性.全工序低氧位控制,减少氧化铝夹杂物的产生.合理地控制RH循环时间和精炼后钢水镇静时间,严格执行保护浇注和控制大包下渣等措施,钢水可浇性大幅提高,实现搪瓷钢连浇炉数由原来3炉提高至6炉. 
 Abstract:Inresponsetothepoorcastabilityofhightitaniumultra-lowcarbonenamelsteelandthetendencyofnozzleclogging,amechanismanalysiswasconductedonthenozzlecloggingandtheircauses.Subsequently,bystrengtheningthetopslagmodification,theoxidationresistanceofthetopslagwasreduced.Lowoxygenlevelcon-trolthroughouttheentireprocesstoreducethegenerationofaluminainclusions.ReasonablecontrolofRHcycletimeandsteelquenchingtimeafterrefining,strictimplementationofmeasuressuchasprotectivecastingandcontrolofslagintheladle,significantlyimprovethecastabilityofsteel,andachieveanincreaseinthenumberofcontinuouscastingfurnacesforenamelsteelfromtheoriginal3to6.
 
 作者:黄传根Author:HuangChuangen
 作者单位:马钢股份公司安徽马鞍山243000
 刊名:安徽冶金科技职业学院学报
 Journal:JournalofAnhuiVocationalCollegeofMetallurgyandTechnology
 年,卷(期):2024, 34(1)
 分类号:
 关键词:高钛  搪瓷钢  水口结瘤  提高可浇性
 Keywords:hightitanium  enamelledsteel  nozzleclogging  improvecastability
 机标分类号:TF777.1TF811TS105.213
 在线出版日期:2024年6月11日
 基金项目:提高高钛超低碳搪瓷钢可浇性生产实践[
 期刊论文]  安徽冶金科技职业学院学报--2024, 34(1)黄传根针对高钛超低碳搪瓷钢可浇性差、水口易结瘤情况,对水口结瘤物和结瘤原因进行了机理分析.后续通过强化钢包顶渣改质,降低了顶渣氧化性.全工序低氧位控制,减少氧化铝夹杂物的产生.合理地控制RH循环时间和精炼后钢水镇静时...参考文献和引证文献
 参考文献
 引证文献
 本文读者也读过
 相似文献
 相关博文
 
 关键词:高钛,搪瓷钢,水口结瘤,提高可浇性,
 
 
 
文件大小:397.81 KB 
下载次数:60 
 
		
高速下载
 | 
 |