| 文档摘要:作为锂离子电池负极材料,金属锡及锡氧化物随锂离子的嵌入与脱出会产生巨大的体积变化,导致循环过程中储锂容量及循环性能急剧衰减.以氯化亚锡(SnCl2)和对苯二甲酸为原料,通过水热法制备了Sn-MOF衍生的金属氧化物@C复合材料.研究结果表明,SC-1样品中的主相SnO2及少量的SnO均匀分布在具有丰富介孔结构的无定形碳基体中,相较于其他两个样品,表现出更好的容量性能、高倍率充放电性能和电化学结构稳定性.SC-1样品在0.1A/g下充电比容量达到1092.4mAh/g,在2A/g下充电比容量仍达到308.9mAh/g,经过100次循环后容量保持率为56.8%. 
 Abstract:Asanodematerialsforlithiumionbatteries,metaltinandtinoxidesundergosignificantvolumechangeswiththeinsertionandremovaloflithiumions,leadingtoasharpdeclineinlithiumstoragecapacityandcyclingperformanceduringthecyclingprocess.Usingstannouschloride(SnCl2)andterephthalicacidasrawmaterials,theSn-MOFderivedmetaloxide@Ccompositematerialswerepreparedthroughhydrothermalmethod.TheresultsindicatethatthemainphaseSnO2andasmallamountofSnOintheSC-1sampleuniformlydistributeintheamorphouscarbonmatrixwithrichmesoporousstructure.Comparedwiththeothertwosamples,itshowsbettercapacityperfor-mance,high-ratechargedischargeperformanceandelectrochemicalstructuralstability.ThechargespecificcapacityofSC-1sampleis1092.4mAh/gat0.1A/g,and308.9mAh/gat2A/g.After100cycles,thecapacityretentionis56.8%.
 
 作者:田光梅   魏润源   王尧尧   王北平 Author:TIANGuangmei   WEIRunyuan   WANGYaoyao   WANGBeiping
 作者单位:北方民族大学材料科学与工程学院,宁夏银川750021金川集团职工培训中心,甘肃金昌737100北方民族大学材料科学与工程学院,宁夏银川750021;宁夏硅靶及硅碳负极材料工程技术研究中心,宁夏银川750021
 刊名:电源技术 ISTICPKU
 Journal:ChineseJournalofPowerSources
 年,卷(期):2024, 48(6)
 分类号:TM912.9
 关键词:锂离子电池  金属氧化物复合材料  水热法  电化学性能
 Keywords:lithium-ionbattery  metaloxidecomposites  hydrothermalmethod  electrochemicalper-formance
 机标分类号:TB332TM912.9TM242:TM205.1
 在线出版日期:2024年7月9日
 基金项目:宁夏自然科学基金项目,北方民族大学研究生创新项目Sn-MOF衍生的多相复合材料的制备及储锂性能[
 期刊论文]  电源技术--2024, 48(6)田光梅  魏润源  王尧尧  王北平作为锂离子电池负极材料,金属锡及锡氧化物随锂离子的嵌入与脱出会产生巨大的体积变化,导致循环过程中储锂容量及循环性能急剧衰减.以氯化亚锡(SnCl2)和对苯二甲酸为原料,通过水热法制备了Sn-MOF衍生的金属氧化物@C复合...参考文献和引证文献